Sheet Metal Tolerances: Bends and Flatness
Sheet metal holds ±0.1 mm (±0.004") on cut features, but bends move and holes near bends distort. Where the real limits sit.

Sheet metal parts are cut flat and bent into shape, and the tolerances that apply to each step are different. A laser-cut hole can hold a tight tolerance; the same hole, bent into a flange, will sit a little differently than the flat pattern says; and a large flat panel will never be as flat as a machined face. The trick is knowing which dimensions can be held tight, which ones move with the bend, and which ones need a separate callout on the drawing rather than a general tolerance.
What ±0.1 mm (±0.004") covers
On cut features — laser-cut outlines, punched holes, slots — a tolerance of ±0.1 mm (±0.004") is the standard we work to. Hole diameters, hole positions in the flat, overall outline dimensions and slot widths all fall in this range on normal sheet metal work. Features that are not called out on the drawing fall under the general tolerance standard, ISO 2768 — see ISO 2768 general tolerances for what applies when a dimension has no tolerance of its own.
That ±0.1 mm (±0.004") does not extend to everything on the part. Dimensions that cross a bend, and flatness of a large panel, are governed by the bending process and need their own numbers.
Bend angles and bend positions
A bend is not as repeatable as a cut. The bend angle depends on the material, its thickness and temper, the tooling, and the grain direction, and the same setup will give slightly different angles on different batches of material. Any angle that has to be exact — a flange that must sit square against a mating part — should be called out on the drawing so it is checked and corrected.
Bend position is also less exact than a cut dimension. The flat pattern is calculated from the bend allowance, and a small error in the allowance shifts every dimension that crosses the bend — see K-factor, bend allowance and flat pattern. If the flat pattern is wrong, the folded part will be wrong, and no amount of careful bending fixes it.
Holes near a bend: keep your distance
A hole placed too close to a bend line will distort when the bend is made. The material stretches on the outside of the bend and compresses on the inside, and a hole caught in that zone comes out oval, or its edge tears. The rule is simple: keep holes a sensible distance from the bend line, and if a hole must sit close to a bend, put it in after bending, or accept that it will need reaming or cleanup.
The same applies to slots and notches near bends. When a hole has to be close to a bend for functional reasons, say so at the quote stage: the shop can plan the sequence, bending first and drilling or punching after.
Flatness: what a panel can and cannot do
A sheet metal panel is never perfectly flat. Rolling leaves a slight curve in the coil, handling adds small waves, and welding or bending adds more. For a large panel, flatness is a matter of degree, and the drawing should say what is acceptable rather than assuming the panel will be dead flat.
Flatness matters most where the panel mounts to something — a cover that must sit flush, a panel with a gasket that must seal, a mounting plate that carries a bearing. In those cases, the flatness callout goes on the drawing with a value, and the shop can check it and correct it. Where flatness is not called out, the panel is made to normal shop practice, which is flat enough for a cover but not for a sealing face. For how bends, holes and flanges should be laid out in the first place, see sheet metal design tips: bend radius, flanges and holes.
Thickness and material variation
Sheet metal thickness itself has a tolerance, set by the mill, and it varies slightly from coil to coil. A part designed around a nominal 2 mm (0.08") thickness will see real thickness a little above or below that. Most features tolerate that variation without a problem, but a stack of parts, or a slot that a mating part must slide into, can be affected. Where thickness matters, the drawing should say so, and the shop will measure the actual coil thickness and adjust the bend allowance.
How tolerances stack up on an assembly
A single part with generous tolerances can still fail in an assembly if every part is at the edge of its tolerance in the same direction. A hole pattern that must line up with a mating part, a flange that must meet a cover, a bracket that must clear a cable — all of these depend on the stack-up, not on any single dimension. The practical fix is to put the tight tolerance on the dimensions that decide the fit, and leave the rest to the general tolerance. A drawing with tight tolerances everywhere costs more to make and is no more accurate where it counts.
What to send for a quote
A drawing with the bend locations, the hole positions and any flatness or angle callouts marked, plus the material and thickness. Dimensions that cross a bend, and any dimension that decides a fit, should carry their own tolerance rather than relying on the general standard. If you want a sheet metal part quoted, send us your drawing — inquiries are answered within 8 hours and quotes usually within 24 hours.
FAQ
What tolerance can sheet metal parts hold? Cut features — laser-cut outlines, punched holes and slots — hold ±0.1 mm (±0.004") as standard. Dimensions across a bend and flatness of large panels are less exact and need their own callouts.
Why do holes near a bend distort? The material stretches on the outside of the bend and compresses on the inside. A hole caught in that zone comes out oval or tears at the edge. Keep holes a sensible distance from the bend line, or put them in after bending.
How flat can a sheet metal panel be? A panel is never perfectly flat — rolling, handling and bending all add small waves. If flatness matters, for a sealing face or a mounting surface, put a flatness value on the drawing so it is checked and corrected.
Does sheet metal thickness vary? Yes, slightly, from coil to coil, within the mill tolerance. Most features tolerate it, but a stack of parts or a slot that a mating part slides into can be affected, so flag thickness-critical features on the drawing.
Why is the flat pattern so important? Because every dimension that crosses a bend depends on it. A wrong bend allowance shifts the folded dimensions, and no amount of careful bending fixes a flat pattern that was calculated wrong.