Picking a material is the first decision on any machined part, and it drives everything after it — strength, weight, corrosion resistance, finish, and cost. This guide runs through the four questions we ask on every quote, then compares the metals and plastics we machine most.
Start with Four Questions
1. How strong does it need to be, and how heavy can it be? Strength alone rarely decides. Aluminum carries most structural loads at a third of the weight of steel; titanium matches steel's strength at roughly half the weight. If the part moves, gets carried, or bolts onto something weight-sensitive, the lighter material usually wins even at a higher price per kilo.
2. What will attack it? Water, salt air, cleaning chemicals, and body fluids all punish the wrong choice. Stainless steel and titanium shrug off corrosion that would eat carbon steel in months. If a carbon steel part is strong enough and cheap enough, a coating can close the gap — but coatings wear, and base metal doesn't.
3. What environment does it live in? Heat rules out most plastics and weakens aluminum. Continuous friction and wear point toward hardened steel or tungsten carbide. Electrical and thermal conductivity point the other way, toward copper and aluminum.
4. What does it cost to buy — and to machine? Material price is only half the bill. A cheap bar of stainless can cost more in cycle time than an expensive bar of aluminum, because it cuts slower and eats tools. The right question is total part cost, and it's one reason we flag material choices at quote stage when a swap would save real money.
The Materials, Side by Side
| Material | Good for | Machining notes | Common finishes |
|---|---|---|---|
| Aluminum alloys (e.g. 6061) | Housings, brackets, plates, enclosures — the default for most parts | Fast to cut, holds detail well; the best strength-to-cost starting point | Bead blast + anodizing (clear or black), powder coating |
| Stainless steel (304, 316, 440C) | Corrosion resistance, food and medical environments, wear parts in 440C | Slower cutting, work-hardens; 316 for harsher corrosion, 440C where hardness matters | Passivation, electropolishing, black oxide (440C) |
| Carbon steel | Strong, low-cost structural parts | Easy to machine; needs a protective finish against rust | Black oxide, zinc or nickel plating, powder coating |
| Copper | Electrical and thermal conductivity — terminals, heatsinks, electrodes | Soft and gummy; needs sharp tools and care with burrs | Usually left bare, or nickel plated |
| Brass | Fittings, connectors, decorative hardware | One of the easiest metals to machine; clean chips, good threads | Usually bare, or nickel/chrome plating |
| Titanium (Ti Gr2, Ti Gr5) | High strength at low weight, excellent corrosion resistance | Slow, hot cutting; Gr2 for corrosion duty, Gr5 where strength counts | Bead blast, anodizing |
| Tungsten carbide (YG10X) | Extreme wear: nozzles, dies, cutting and forming edges | Not milled conventionally — shaped by EDM and grinding; lead time around 20–30 days | Ground finish as standard |
| Engineering plastics (POM, PEEK, Nylon) | Light, insulating, low-friction parts; PEEK for heat and chemicals | Fast to cut but flexible — thin walls and tight flatness need care | Usually as-machined; painting and printing on request |
A few of these deserve a closer word.
Aluminum is where most projects start, and often where they should stay. It machines quickly, anodizes beautifully, and covers a wide range of structural work. Move away from it when you need steel's wear resistance, copper's conductivity, or a plastic's insulation — not by default.
Stainless steel is really three decisions. 304 is the general-purpose grade. 316 adds molybdenum for chloride environments — marine air, medical, food processing. 440C is the one that hardens: it trades some corrosion resistance for the hardness that shafts, knobs, and wear surfaces need, and it takes a black oxide finish well.
Tungsten carbide is the specialist. Our carbide work is all YG10X — density 14.3 g/cm³, hardness 91.6–91.8 HRA, average grain size 0.8 µm, bending strength above 2700 MPa. Nothing else on this list survives abrasive wear like it, but it can't be milled or turned the normal way; it's ground and EDM-cut, which is why carbide parts run on a longer lead time. Our tungsten carbide parts page has the details.
Engineering plastics split by temperature and budget. POM (acetal) is the machinist's plastic: stable, slippery, easy to hold to tolerance. Nylon is tougher and cheaper but absorbs moisture and moves with it. PEEK is the high-end answer — it keeps its properties at temperatures that soften the other two and resists most chemicals — at a material price to match.
Pairing Material with Surface Finish
Finish choice is partly a material question, because not every finish works on every metal:
- Anodizing is aluminum-only (titanium takes a thinner decorative version). It's our most common finish: bead blast first for an even matte surface, then clear or color anodize.
- Passivation is stainless steel's finish — it restores the corrosion-resistant surface after machining without adding a layer.
- Black oxide suits carbon steel and 440C stainless: a thin black conversion coating that barely changes dimensions.
- Plating — nickel, chrome, zinc — adds a metal layer for corrosion protection, wear, or appearance on steel, brass, and copper.
- Powder coating covers aluminum and steel when the part needs a tough, colored, non-conductive skin.
The full menu, with standards, is on our surface finishing page. If you're unsure which finish your material and environment need, ask at quote stage — it's much cheaper to choose on paper than to refinish parts.
FAQ
What material should I choose for a first prototype? Start with the material you intend to produce in, if it's machinable — prototypes in a substitute material can hide fit and strength problems. If cost forces a substitute, 6061 aluminum is the usual stand-in for metal parts and POM for plastic ones.
Can you help me choose if I'm not sure? Yes. Tell us what the part does, what it bolts to, and what environment it lives in, and we'll recommend a material and finish with the quote. We'd rather argue about materials before cutting than after.
What tolerances can you hold in these materials? Standard tolerances are ±0.1 mm across our CNC machining and CNC turning work, with ±0.01 mm available on critical features. Plastics and thin parts may need the tolerance plan discussed feature by feature — flexible materials don't hold numbers the way metal does.
Do you provide material certificates? Yes — material certificates, FAI reports, and a certificate of conformance are available on request. Say so when you send the drawing so they're prepared with the order, not chased after it.
Why does tungsten carbide take 20–30 days when other parts take 3–5? Carbide can't be cut with normal milling and turning; it's shaped by EDM and precision grinding, which are slower processes on specialized machines. Standard metal and plastic prototypes typically ship in 3–5 days.
Not Sure? Send the Drawing Anyway
You don't need the material settled before asking for a quote. Send the drawing or 3D model, tell us what the part has to survive, and we'll come back within 24 hours with a price and an honest material recommendation — including when the cheaper option is the right one. We reply to every inquiry within 8 hours, and we're happy to sign an NDA before your drawings change hands.